Backscatter Imaging Figures
Figure 1
Backscattered electron image (35 kV) of metal voiding in a power bus caused by electromigration.

Figure 2
Diagram showing the electron beam physics interaction volume.

Figure 3
Backscattered electron image (35 kV) showing voiding in the metal 1 layer in this two level metal IC (Photo courtesy Analytical Solutions).