Optical Examination I Figures
Figure 1
Photograph of a diffusion pipe that produced a collector emitter short on a bipolar technology. (Courtesy DM Data).

Figure 2
Cross sectional view through a bond wire / bond pad interface showing intermetallics. (Courtesy DM Data).