Liquid Crystal Analysis Figures

Liquid crystal analysis showing a hot spot on a memory IC. (Courtesy DM Data).




Metal to metal shorts identified by liquid crystal analysis on a 64k EEPROM. (Courtesy Sandia Labs).




Example of a hot spot on an IC die detected with liquid crystal. (Courtesy Analytical Solutions).




Example of a thin oxide defect on an IC detected with liquid crystal. (Courtesy Analytical Solutions).




Liquid crystal showing a hot spot metal to metal on the same layer. (Courtesy Sandia Labs).